A model of focused ion beam deposition of materials is described. Decomposition of
organometallic molecules by ion beams 50-300 nm in diameter allow localized deposition
of a variety of metals. The large current density (approximately I A/cm2) and
the inherent sputtering of a focused ion beam can result in no net deposition for a
variety of process conditions. The major process parameters of current density, beam
dwell time, and readsorption time are introduced. Experimental examples of gold
depositions from dimethylgold hexafluoro acetylacetonate or DMG(hfac) are presented
to illustrate the effect of the process parameters on size and shape of the
depositions.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
For repairing opaque defects on x-ray masks by focused gallium ion beams (Ga-FIB), it is
important to achieve nearly vertical slopes in the remaining absorber material and to avoid the
redeposition of sputtered particles. The sputter yield depends on the angle of incidence. Since this
angular dependence influences the slope angle, th sputter yield of a 100 keV focused Ga ion beam
on polycrystalline gold, as used on x-ray masks, was measured at five different angles of incidence
(8 =0 , 30 , 45 , 60 , 80 ). At normal incidence (9 =0 ) the yield is 32. It increases with increasing
angle of incidence and becomes 128 at e = 80
By means of computer simulations it could be shown, that the sputter yield at great angles of
incidence plays the predominant role for the evolution of the slope, even if the repair process is carried
out with nominally vertical incidence. A high sputter yield at a great angle of incidence leads to a
precipitous slope (a =85 ). An even better slope angle was achieved when the beam was scanned in an
appropriate manner: If the center of the beam, where the ion current density is maximum (Gaussian
beam shape), is directed onto the lower parts of the slope, there, an increased sputter erosion takes
place. The reason is not only the increased ion current density, but the higher sputter yield at great
angles of incidence as well. Experimentally and in a computer simulation it could be shown that a slope
angle of a =88 can be achieved in forward direction (direction of scanning).
Since redeposition affects the microstructuring of gold substantially, the redeposition characteristics
(spatial distributions of sputtered particles) were measured for two angles of incidence (=0 , 45°). In
both cases an area of 500 zm x 10 mm of a polycrystalline gold layer was bombarded with a 100 keV
Ga+ focused ion beam. The sputtered particles were collected on semi-cylindrical glass screens. The
redeposited gold layers on the inner surface of the glass screens were measurable after 40 hours of
sputtering each specimen. The maximum thickness was 1.4 nm for the normal incident beam and 2.2 nm
for a beam inclination of 45 . The redeposited layers were evaluated locally resolved by an optical
transmission measurement system. These measurements show that the spatial distribution of the sputtered
gold particles can be approximated by a cos2-function for both, normal and inclined incidence. Taking
this distribution, the simulations were carried out.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
A 25 key focused Ga ion beam was used to induce deposition
of tungsten on a gold absorber on boron nitride X-ray mask with
submicron features to simulate the repair of clear defects.
Tungsten was deposited to fill holes, extend lines and add
missing features, such as isolated contacts and lines. Deposits
were placed between features and made to cross over both gold
and tungsten features to evaluate proximity effects. Series of
tungsten depositions that varied in thickness were exposed to an
X-ray source and transferred into resist. Contrast equivalent
to or better than the gold absorber was achieved for tungsten
that was thinner than the gold.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
This paper describes recent developments in three areas ofmasked ion beam lithography (MIBL). These are 1) fabrication
oflarge area, low distortion, silicon stencilmasks for demagnifying ion projection lithography, 2) fabrication ofstencil masks
with nanometer scale resolution for 1:1 proximity printing, and 3) development of a direct method of alignment using the
ion beam induced fluorescence of Si02. These topics are discussed below.
Demagnifying ion projection masks: We describe the fabrication of stencil masks in large area, low stress (10 MPa), n-type
silicon membranes. The projection masks have a silicon foil area 95 mm in diameter, thicknesses between 1.5-5 and
resolution of0.6um. Measured distortion (3a) in the IPL masks ranges between 0.23gm and 0.65,um, with an experimental
error of 0.20 1um.
Proximity printing masks: A process is described for fabricating stencil masks with 50 nm resolution in low stress, n-type
silicon membranes. Membranes less than 0.5 ,ttm thick are shown to be free of the sidewall taper that limits resolution in
thicker masks. These thin membranes show a slightly flared profile due to the imperfectly collimated etching ions.
Alignment: A direct method of alignment is being developed which uses the ion beam induced fluorescence of Si02 marks.
Fluorescence yield is characterized as a function of ion energy and resist coating thickness. The yield for Si02 is in the range
between 0.1-1.0 photons/proton, while the yields for Si, Al, and photoresist are negligibly small. Thus, a simple alignment
technique can be implemented where registration of a grating in the mask with a corresponding oxide pattern is detected
as a fluorescence maximum. A simple model predicts that 50 nm alignment can be accomplished, following a 1 im
prealignment, in 2 seconds.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
High-resolution patterning of thin-film high temperature superconductors is necessary in the development
of device applications of these new materials. Such fine-line structures are necessary in the fabrication of
devices such as superconducting quantum interference devices (SQUIDs), transmission lines and others.
Furthermore, high spatial resolution patterning can be an important tool in studying the fundamental
properties of the films themselves. Focused ion beam patterning has recently been applied to YBaCuO
thin films. The finely focused ion beam can produce patterns by local physical sputtering or through
implant damage. These techniques have proven to be valuable for producing submicron superconducting
structures in a reliable way. This paper describes the method of modification and patterning of high T
thin films by focused ion beam implantation damage. For low ion doses, the film properties such as
critical current and transition temperature are reduced monotonically with dose. At higher doses, the
material is rendered non-superconducting locally. We show that micron-sized superconducting structures
can be fabricated by this very simple one-step technique at ion doses in the range of 1012 to iO"1 ions/cm2
with a 300 keY Si beam.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Dielectric breakdown of gate oxide by the focused iou beam (FIB) irradiation of the MOS structure has
been studied. The sample device structure was that of an MOS transistor about to be ion-implanted in the
source and drain (S/D) regions. The gate poly-silicon electrode was extended to the pad electrode on the thick
field oxide. The thicknesses of the gate and field oxide layers were 25 iim and 500 mu, respectively. That of
the poly-silicon layer was 250 nm. The typical areas of the gate and the pad electrodes were 31-100 jzm2 aiid
2-4x iO pm2, respectively. Gallium FIB, accelerated by 40 keV, was irradiated to sample devices.
The total dose until the breakdowii depends on the irradiated location of the device. In the case that the
edge of the polysilicon layer adjacent to the S/D regions is irradiated, the dose is the least. If the gate oxide
layer has not been removed on the S/D regions, the dose exceeds that for the sample with the gate oxide layer
etched there, although not greater than that in the case that any other part of the poly-silicon layer is irradiated.
The electroluminescence measurement of some samples indicates that such edge irradiation iiiduces damages at
a spot on the irradiated edge of the gate oxide. Such damages are probably due to the combiiiation of conductive
microbridge formation and the electrical dielectric breakdown around the bridge. The microbridge is formed
by the implantation of gallium ions, and/or adhesion of gallium and silicon atonis at the sidewall of the gate
oxide. In the experiments where an area around the center of the polysilicon pad electrode was irradiated, two
breakdown modes were observed: breakdown due to gate-culTent stress and instant breakdown.
The gate potential during the FIB irradiation was obtained from the measured secondary electron current.
The potential is approximately equal to that measured during the conventional constant-current-stress (005)
lifetime experiment. This proves that gate oxide is stressed by current during irradiation. The time to breakdown
becomes shorter with decrease in the gate area if the FIB current is the same. The smaller the devise becomes,
the 005-like mode will be the more serious.
Instant breakdown mode appears when the beam current is high. Detailed analysis reveals discrepancies
between the phenomena and simple conjectures based on the 005 lifetime. By the irradiation, some samples are
broken in far shorter time than expected from the 005 lifetime measurement, whereas the rest of the samples
survive longer than the expectation. This suggests that there is a stronger stress at the onset of the irradiation.
This breakdown mode is, at least at present, uncontrollable and most hazardous, to be overcome for improved
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The exposure characteristics of polymethyl isopropenylketone(PMIPK) and polyphenyl -
isopropenylketone(PPIPK) exposed to 40 and 80 KeV H+ and B+ ion-beam have been
studied. It is believed that the electron rich phenyl group in PPIPK has increased
stopping power to bigger B ion, but not to smaller H+ ion. Linear relationship is
found with simulation parameter A as a function of exposure dose (KeV x ion fluence)
for specific ion and polymer within the used energy range. Gel permeation
chromatography also indicates that the main chain scissioning of PMIPK is faster than
that of PPIPK when they are exposed to B+ under same exposure conditions.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Projection and proximity printings are compared in terms of linewidth tolerance. Computer
simulated exposure-defocus and gap-exposure diagrams are used to characterize the two techniques
respectively. The depth of focus for projection printing in terms of the universal depth
parameter k2 is evaluated as a function of the universal width parameter k1, for five long and
short representative lithographic features, then three long features. Similarly, the depth of focus
and working distance for proximity printing are evaluated for a O.25-jm system in x-ray and
2.5-,um system in uv and some preliminary comparison to experimental results is shown. The
image contours and depth of focus of the two imaging techniques are compared. Proximity
effects are present for both techniques. The distinction of working distance and depth of focus
for proximity printing is observed for the first time. Against intuition, a shorter mask-to-wafer
gap is not always better.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Little work has been performed to characterize the exposure sensitivity, contrast, and tone of
candidate resists for photon energies between 100-300 eV, the range in which projection soft x-ray
lithography will be developed. We report here the characterization of near-edge x-ray absorption fine
structure (NEXAFS) spectra, exposure sensitivity, contrast, and post-exposure processing of selected
polysilane resists at photon energies close to the Si L2,3 absorption edge (100 eV). We find absorption
resonance features in the NEXAFS spectra which we assign to excitation into Si-Si and Si-C *orbitals.
Using monochromatized XUV exposures on the Si-Si cs* resonance at 105 eV, followed by solvent
dissolution development, we have measured the exposure sensitivity curves of these resists. We find
sensitivities in the range of 600-3000 mJ/cm2 and contrasts in the range from 0.5 - 1.4, depending on the
polysilane side chain. We have also performed exposure sensitivity measurements at 92 eV, below the
edge. Sensitivity decreases slightly compared to 105 eV exposures and the saturation depth and contrast
both increase, as expected. We find also that exposing resist films to oxygen after XUV exposure, but
before development, increases the sensitivity markedly.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The comment that typical clean room 'soft' defects (i.e., airborne, carbon-based
particles) are transparent to x-rays is stated as a fundamental attribute of x-ray
lithography. However, data showing lithographic conditions which result in a reduction
in defect density have not yet been widely published. This paper reports an
analysis of defect printability for soft x-ray lithography at wavelengths of 0.6 to
2.2nm and denotes exposure and resist development conditions under which representative
soft and 'hard' reticle defects did not print. Resolution reticles with features
down to 0.5pm were produced using Hampshire's baseline process which consists
of electroplated gold absorber on a silicon support membrane. Latex spheres ranging
in diameter from 0.36 to l.Opm were applied by VLSI Standards, Inc. to simulate soft
defects. The large exposure latitude for x-ray lithography allows using an overexposure
to reduce the impact of lower contrast defects without appreciable CD change.
The printability of soft defects and defect-induced wall angle perturbations in
resist patterns were also investigated through simulations using a modified version
of SAMPLE and the results agreed with the observations. Identification of what constitutes
a printable reticle defect for x-ray lithography is not as straightforward
as that for optical lithography.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Target X-ray source lithography and photo lithography mixed and match system was proposed for
an effective lithography system. The key technology for the system is a projection moire
alignment, whose marks are used for both photo and X-ray lithography. In order to realize the
systeimi, related technologies and apparatus are developing, which are photo and X-ray stepper, Xray
source of radiation cooled slotted Pd target, X-ray mask and X-ray mask inspection system.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Synchrotron radiation from dipole magnets in electron storage rings has emerged as a useful source of x-rays for
lithography. To meet the need for these sources numerous groups around the world have embarked on projects to design
and construct storage rings for x-ray lithography. Both conventional electromagnets as well as superconducting (SC)
dipoles have been incorporated into the various designs. An overview of the worldwide effort to produce commercial xray
sources will be presented. To better illustrate the elements involved in these sources a closer examination of the
Superconducting X-ray Lithography Source Project (SXLS) at BNL will be presented.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Synchrotron radiation from electron storage rings has the unique
capacity to provide the several kilowatts of continuous X-ray power
necessary for production scale X-ray lithography-. While national
laboratories have developed electron storage ring technology to an
exact science and can provide X-ray beams of an intensity and
quality appropriate for lithography, they have not built machines
optimized for lithography and designed to be replicated in
semiconductor fabrication facilities. Since 1983, Oxford
Instruments have been working on the development of a practical
synchrotron X-ray source, called Helios. Final system tests will
commence this spring on the initial Helios compact synchrotron.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
In the previous paper, you heard a description of the electron storage ring
system that IBM has ordered for X-ray Lithography. In this paper we shall
describe the facility that is being constructed for the ESR and explain some of
the decisions made in its design.
The facility, which we have dubbed ALF for Advanced Lithographic Facility,
is a part of the $O.5B Advanced Semiconductor Technology Center now being
occupied at IBM's East Fishkill, New York semiconductor plant. Ground was
broken in October of 1988 and the ALF building is expected to be ready for
occupancy in July of this year. At that time, initial preparations for
installation of the ESR and the lithographic tooling will begin. Bechtel
National of San Francisco is the Design-Build contractor.
As you may have concluded from Dave Andrew's paper, an ESR and its
associated cryogenic, cooling, power and control systems is a complex tool which
requires specialized support. In addition, the facility must support the
vibration control and clean room requirements of submicron lithographic
processing. Also, significant concerns of safety and security must be met. We
will now describe our solutions to these requirements.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The electron storage ring is a realistic solution as a radiation source for production grade, industrial X-ray lithography
system. Today several large scale plans are in motion to design and implement synchrotron storage rings of different types for
this purpose in the USA and abroad. Most of the scientific and technological problems related to the physics, design and
manufacturing engineering, and commissioning of these systems for microlithography have been resolved or are under
extensive study. However, investigation on issues connected to application of Synchrotron Orbit Radiation (SOR ) in chip
production environment has been somewhat neglected.
In this paper we have filled this gap pointing out direct effects of some basic synchrotron design parameters and
associated subsystems (injector, X-ray beam line) on the operation and cost of lithography in production. The following
factors were considered: synchrotron configuration, injection energy, beam intensity variability, number of beam lines and
wafer exposure concept. A cost model has been worked out and applied to three different X-ray Lithography Source (XLS)
systems. The results of these applications are compared and conclusions drawn.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Two major categories of electron beam lithography systems have been developed over the
course of many years: Direct write of chips on silicon, and patterning of optical masks on
quartz and glass substrates. This paper addresses this dual role and what it implies for the
different classes of electron beam lithography tools. In direct write, with dimensions at and
below 0.25 m, tool resolution, accuracy in registration and overlay, process integration, and
other factors are of critical importance. Most recent advances in this area will be described.
Current work on device fabrication below 0.25 ,um demonstrates the capability to integrate all
sectors of electron beam lithography to provide early research work for ULSI device technology
demonstration. These dimensions are necessary for the fabrication of 256 MB DRAM chips,
for example.
For mask making it is widely ackowledged that much of the learning from direct write electron
beam lithography tools becomes applicable to mask patterning as well. However, more stringent
requirements are burdened in particular on x - y stage accuracy and long term overall
systems stability.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The use of E-beam lithography for direct writing GaAs device levels is a widely accepted technique in the manufacture of
discrete PET and MMICs. Throughput in these applications is a function of wafer size, number of chips, resist sensitivity,
available beam current, pattern density and the inherent tool overheads of stage movement and registration time. Of these,
chip registration can be the single most time consuming component. Techniques have been developed that minimize the
writing time while maintaining the required level and pattern accuracy. These techniques include using multiple beam currents
and multiple field sizes for high and low resolution areas and using optical exposure of less critical areas in a mixed
lithography scheme. In this paper we present a technique of cluster registration that reduces registration time by as much as
75 percent. Resultant data illustrate no loss of line width control or placement accuracy utilizing this procedure. We describe
software techniques and procedures that provide automatic creation of job control files and system executive control files
yielding full turn key operation of a Cambridge EBMF 10.5 E-beam pattern generator. In addition, we discuss the use of this
lithography tool for automated line width metrology of the resultant lifted off gate.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The proximity effect, caused by electron beam backscattering during resist exposure, is an important
concern in writing submicron features. It can be compensated by appropriate local changes in the incident
beam dose, but computation of the optimal correction usually requires a prohibitively long time. We present an
example of such a computation on a small test pattern, which we performed by an iterative method. We then
used this solution as a training set for an adaptive neural network. After training, the network computed the
same correction as the iterative method, but in a much shorter time. Correcting the image with a software based
neural network resulted in a decrease in the computation time by a factor of 30, and a hardware based network
enhanced the computation speed by more than a factor of 1000. Both methods had an acceptably small error of
0.5% compared to the results of the iterative computation. Additionally, we verified that the neural network
correctly generalized the solution of the problem to include patterns not contained in its training set.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
it is essential to avoid charging effects in E-beam direct writing for the
fabrication of deep-sub-micron devices. It has been found that a spin-coated
surfactant layer over the imaging resist can avoid charging effects. Application of
this method to multilayer resist process is presented. With optimum surfactant layer
thickness. there is no influence of surfactant layer on resist sensitivity or
resolution. The surfactant layer can be removed easily in imaging resist development
p r o c e
In the case of tn-level resist with a 2.4pm overall thickness. registration
error was reduced from I. 0 jim to 0. 1 um( isv. i +26) by adding a 0. l2,um-thick surfactant
layer. Quarter micron patterns with good profiles were achieved using CMS-EX(R) as
the imaging layer.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
This paper will outline a novel technique for fabricating T-gates. Although dependent upon two
lithographic exposures, this process is more robust and flexible than existing techniques. The
resultant gates are structurally stable, with electrical resistance that can be made arbitrarily
small by increasing the size of the T-gate top. Moreover, this gate process is fully compatible with
existing MESFET and HEMT fabrication methods.
Performance of microwave devices will be presented, contrasting 0.25 tm conventional gates
with vacuum passivated T-gates. The T-gates will be shown to offer superior breakdown and gain
performance and to produce FET characteristics which remain stable from gate level to final frontside.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Electron-beam lithography was used to fabricate half-micron, quarter-micron and sub-quartermicron
gates for MMIC applications. Both rectangular and mushroom gates were used. This paper
describes our experience in the fabrication of various gates, with emphasis on obtaining good
reproducibility and high yield. For optimum utilization of machine time, the operating condition of the
exposure system was maintained at 30 kV and 1 .6-mm field size for most applications. In the case of
extremely fine gates of 0. 1 .tm or less, the accelerating voltage used was 40 kV. Gates with excellent
reproducibility and yield of □ 90% were obtained.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The distortions that arise from thermal stresses in X-ray masks which employ the embedded
absorber structure are modelled and analyzed. By using a quasi two-dimensional model, both in-plane
and out-of-plane distortions were characterized and their dependence on the fractional absorber
coverage was calculated. These distortions were found to be large when the absorber was initially
deposited at a high temperature; however they can be greatly reduced by adding a buffer layer between
the absorber and membrane. The Young's modulus and the linear expansion coefficient of this buffer
layer are chosen such that the mask distortions are compensated for. Without the buffer layer, the shear
and peeling stresses at the absorber-membrane interface were found to increase exponentially with
distance near the absorber edges and may cause fatigue. These results were found in agreement with
computer simulations.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Diamond is well suited as an x-ray mask material because of its high x-ray and visible radiation
transparency and exceptionally high mechanical stiffness. This paper presents the optical, x-ray and
morphological properties of a diamond membranes produced on 100mm diameter silicon wafers.
Microwave Plasma Chemical Vapor Deposition was used to deposit diamond films on 1 00 mm diameter
silicon then back-etching the substrate to form taut 75mm diameter free standing membranes. Raman
spectroscopy and x ray diffraction indicates that the films are diamond. X ray diffraction reveals that the
films are fine-grained polycrystalline diamond with a grain size of about 20-30 nm and a [220] growth
texture. The films contain microcrystalline graphite and non-carbon diamond as indicated by the broad
bands at 1355 and 1560 cm, respectively. The FWHM ofthe main diamond peak is relatively
broad,8-1 2 cm , indicating a small crystallite domain and strained microstructure, consistent with the x
ray diffraction data. The measured x-ray transparency of a 3.25M thick membrane at the Cu Ka line is
99.5% while the optical transparency at the He-Ne laser line is 45 %, uncorrected for reflection losses
from both surfaces, absorption and scatter. The transmission in the IR is at the theoretical limit, 71%.
The surface roughness, measured with a sub-micron stylus type profilometer, is about 30 nm rms on the
side away from the silicon substrate and 20 nm on the side adjacent to the substrate. The stress in the
films is tensile with a value of 0.1 1 GPa. The films contain less than 1% hydrogen as determined by
nuclear reaction analysis.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
We report improvements in optical and mechanical properties of x-ray lithography masks based on polycrystalline
Si membranes. The optical transmittance of polycrystalline Si was increased to match that of single crystalline Si in 0.6
to 0.9 j.tm spectral range. This was accomplished by modifying deposition temperature and gas composition during
LPCVD film growth. The new films are intrinsically tensile, allowing formation of taut membranes on crystalline Si
substrates and on glass disks that are matched in thermal expansion to Si, in contrast to earlier polysilicon films which
required thermal expansion mismatch. The mechanical integrity of the masks was further improved by direct deposition of
Si on thick machined glass disks, thus eliminating bonding of thin substrates to rigid support rings. The monolithic
mask blanks are considerably more flat than the bonded structures, either single- or polycrystalline.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The X-ray absorption and mechanical properties of gold containing (Au-C) absorber
formed on polyimide membrane for X-ray lithography mask have been investigated. The
Au-C films were deposited by the same method as the previous investigators(Itoh et
al.)1.
(1) The compositional dependence of film stress before and after the exposure to
SOR radiation has been observed. As a result, the stress in film changed monotonically
ranging from compression (-3xlO8N/m2) to tension (l.2xlO8N/m2) with increasing
Au content. Zero film stress was observed at Au atomic composition of 30%. Films
originally being compressive (-l.5xlO7N/m2) were found to become tensile
(l.OxlO8N/m2) after absorbing l500J/cm3 X-ray. This tendency differs from that of
the BN film observed by King et al
(2) X-ray absorption ratio in Au-C films were determined by measuring the amount
of reduced thickness of resist on development after the exposure of X-ray through
Au-C films with various composition ratios. It was found that it tended to fall from
92% to 68% with a decrease of Au atomic composition ratio from 0.85 to 0.11 at the
constant absorber thickness of 0.5 pm.
(3) Au-C films of various atomic composition ratio were patterned with EB lithography
using the PMMA(Polyrnethylmethacrylate) resist and Reactive Ion Etching (RIE)
with 02 gas. It was found that the etching rate of the film decreases with increasing
Au content. The typical obtained value was approximately 100A/min at around 50%
to 60% of Au composition and this was about 4 times higher than etching rate of pure
Au.
It is concluded that the Au-C absorber on polyimide membrane X-ray mask is practical
for VLSI use for submicron pattern fabrication.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
This paper describes a set of empirical correlations between bulk
resist properties and fine line iniaging quality in an Advanced
Negative e-beam Resist (ANR) . At the on set of this study, it was not
clear whether bulk properties, such as contrast, could be used to
predict image quality. Consequently, several definitions of contrast
have been examined and compared with imaged structures at four unique
processes. These processes were selected based on the results of a
modified Taguchi1 L9 experimental design. The slope of the line
intersecting the thickness response curve at zero percent and ninety
percent retention provides the best correlation with image quality.
This bulk parameter is recommended as a suitable nionitor for sub-half
micron e-beam ANR image quality in 2.38% TMAH.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Copolymers of maleic anhydride with styrene, ethylene, and methyl vinyl ether were modified and
evaluated for use as negative working resist materials in electron beam lithography. The copolymers used
were modified by reaction with an organometallic compound, which resulted in incorporation of tin in the
pendant chains of the copolymers. The polymers were blended with a reactive plasticizer, dipentaerythritol
pentaacrylate (DPEPA), to enhance sensitivity and to improve resolution. The esterified copolymer of
styrene and maleic anhydride was fractionated to obtain fractions with a range of molecular weights and
dispersities. The fractions obtained were used to determine effects of molecular weight and dispersity of the
base polymer on sensitivity and contrast of the resist. The lithographic response of the modified copolymers
was compared with that of the original unmodified base copolymer. Incorporation of tin into the copolymer
resulted in an increase in sensitivity to electron beam. It also improved the dimensional stability of the resist
material. There was a dramatic increase in oxygen reactive ion resistance by incorporation of tin, which was
a result of formation of an etch-resistant passivating barrier. The etch resistance of the tin modified
copolymer containing approximately 20 weight % tin was about twenty fold higher than that of poly(methyl
methacrylate) under identical etching conditions. Blending the polymer with dipentaerythritol pentaacrylate
resulted in a twenty fold increase in electron beam sensitivity over the base copolymer. Tin modified
polymers blended with this plasticizer yielded sensitivities in the range of 0.2 to 1 .5tC/cm2. Fractions of
copolymer obtained were blended with DPEPA and evaluated for lithographic properties. Increase in
molecular weight of the base polymer results in increase in sensitivity of the resist. Monodisperse polymers
yielded higher contrast and better resolution. The effect of molecular weight of base copolymer on contrast
was determined independent of molecular weight distribution.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
A new positive working system for e-beam lithography, called
PRIME (Positive Resist IMage by dry Etching) is proposed.
High contrast (about 6) and resolution 75 nm L/S in O.351um
thick resist are achieved. Very steep profiles can be obtai-
ned on thick resist even at low accelerating voltage as
O.2pm hole in l.2pm thick resist at 20 keV.
To be able to quantify both intra and inter proximity effect
on positive tone resist specific two layers electric tests
chips were designed.
Then PRIME process has been compared, in terms of proximity
effects magnitude, at 20kV and 50 kV, to RAY-PF resist show-
ing clearly advantages over such three components novolac ba-
sed positive resist.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The performance of a new positive tone novalac-based resist, SYSTEM-9, has been characterized on a
Cambridge Instruments EBMF-1O.5 electron beam lithography tool. Resist characteristics and the optimum
processing conditions for a variety of commercially available developers have been investigated. This resist
yields relative contrasts of up to 14, sensitivities from 19 to 32 (jtC/cm2) and a good resolution of 0.2 jim.
SYSTEM-9 has excellent dry etch resistance. Outstanding applications in submicron micro-electronic device
fabrication are demonstrated.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Projection moire alignment is a highly useful technique for mix and match lithographic system. The
same alignment marks are used for both photo and X-ray photolithography and high sensitivity is
obtained using simple alignment optics. This paper deals with a projection moire alignment system
which applies to a g-line or i-line stepper that is part of a mix and match lithographic system. A He-Ne
laser is used as the light for alignment. By using two pairs of gratings which are 1/2 grating pitch out of
phase with each other, we obtain two moire signals which are also 1/2 grating pitch out of phase. Using
difference of these two moire signals, high sensitivity is obtained. In order to achieve high overlay
accuracy in automatic alignment, it is important to consider the shape of the alignment marks.
Asymmetrical resist coverage caused by spin coating causes an offset error and in case of aluminum
coated wafers, a rough surface causes a random error. Some defects in the gratings caused during
etching process also produce error. For the purpose of analyzing some effects of alignment marks on
projection moire alignment, we calculated alignment error using Fresnel diffraction integral. We obtained
the following results. An aberration method using reflected light from wafer marks is useful for rough
surfaces. Defects in a grating are eliminated by average effects. And we calculated an alignment error
caused by wafer tilt. By tilting 5 second to 10 second, output waves become asymmetry and contrast is
reduced. Tilt of 5 sec. makes an alignment error of about 0.03 tm.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
SEM metrology is used to characterizecritical dimension (CD)controlandprocess bias in x-ray reticle fabrication. The
pattern transfer bias between the single layer resist stencil and'the electroplated absorber is investigated. This bias includes the
resist sidewall angle, the accuracy of the SEM edge detection algorithm, and the wet chemical etchants used to delineate the
absorberpattern. It is a well known fact that the resist geometry plays an importantrole in producing the final absorber structure.
Thispaperexplores theeffects ofresistprofilesand subsequentprocessing steps on critical dimension control of the absorber layer.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
The design concept on X-ray lithography system using the X-ray source with an ebeam
excited rotating target has been presented in the previous reportsl The X-ray
source is developed to fit the laboratory and test productive use for the
microlithography applied to O.25iim feature size.
The e-beam focus diameter of 3mm at the power of 3kW to generate characteristic
X-ray of 4.4A(Pd:Lc) wave length has been recently obtained, though it is not satisfactory
as compared with the desired value of 1mm at the power of 10kW.
The fundamental data for this experiment such as the vibration severity with the
rotation of cooling fins, the temperature rise of the target and the maximum voltage
of e-beam without a discharge are discussed. These show that the system will satisfy
a stable structure and cooling capacity enough to step up the e-beam power and to
reduce the spot size of e-beam.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Tanya E. Jewell, M. M. Becker, John E. Bjorkholm, Jeffrey Bokor, Ludwig Eichner, Richard R. Freeman, William M. Mansfield, Alastair A. MacDowell, M. L. O'Malley, et al.
We demonstrate nearly diffraction limited printing using soft x-ray radiation of approximately 36
and 14 nm wavelength. As an imaging system we used a-20X-reduction Schwarzschild-type objective
with iridium coated mirrors for use at 36 nm and Mo/Si multilayer coated mirrors for use at 14 nm.
An off-axis aperture and illumination were used to eliminate the central obscuration in the imaging
system caused by the primary mirror. Two types of masks were used for exposures: an open-stencil
one for 36 nm and a silicon membrane with a Ge absorber for 14 nm. The high absorption of carbonbased
polymers at these wavelengths requires that imaging resist be very thin. Thin resist layers are
not robust and, by themselves, not very useful for processing. By incorporating them into a tn-level
resist, however, we have exposed, developed, and transferred features as small as 0.1 jm into silicon.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
Formation of fine conductive layer patterns by focused ion beam ( FIB ) using
tungsten hexacarbonyl [W(CO)6] has been carried out to study its deposition
mechanism. The effects of beam current density on the deposition rate, using a
chamber-type gas delivery system and a nozzle-type system has been
investigated and compared. It is found that the amount of dependence of
deposition yield on current density differs between the two systems. In addition,
the difference in gas pressures of the two systems cause different compositions
of the deposits.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.