The paper documents a novel method for characterizing pitting corrosion damage in structural materials such as Al 2024-T3. Specimens of such alloys are corroded in a controlled environment and the pits' geometry is captured digitally using white light interference microscopy. The digital data are then processed with wavelet-based analysis thus making possible a multi-resolution description of the geometrical features. The analysis reveals several interesting features of the pits that are similar for all the experimental data analyzed herein, and independent of the process followed for creating them. The first property identified as common to all pits is their geometrical scaling with a (Hurst) exponent of 0.63 +/- 0.12. Furthermore, the ratio (omega) of the surface area of the pit as represented at coarse scales through the wavelet representation, over the area of its intersection with the plane at zero depth is found to be 1.17 +/- 0.07 consistently. The ratio of the total surface area over its intersection is found to be 1.6 +/- 0.2. Either one of these ratios together with the Hurst exponent provide sufficient information for obtaining a pit's geometry from images capturing its 2D shape only, a capability important for efficient characterization. Additionally, such a characterization is paramount for rigorously addressing fatigue crack initiation and propagation.
© (1999) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
George N. Frantziskonis, Laura B. Simon, J. Woo, and Theodore E. Matikas "Characterization of pitting corrosion damage through multiscale analysis", Proc. SPIE 3585, Nondestructive Evaluation of Aging Materials and Composites III, (8 February 1999); https://doi.org/10.1117/12.339869
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Wavelets

Corrosion

Wavelet transforms

Aluminum

Scanning electron microscopy

3D image processing

Microscopes

Back to Top